Grade Comparisons

Side by side

Quick Answer

Grades that look identical on the yard floor can differ by several points of iron, molybdenum or niobium. Each comparison shows what separates two grades and what to check on XRF.

Comparisons

Commonly Confused Grades

Open a comparison for composition side by side, where each grade is used and the reading that settles it.

Inconel 625
Inconel 718

Inconel 625 vs Inconel 718

Inconel 625 is a solid-solution nickel-chromium-molybdenum alloy (about 9% Mo, under 5% Fe) chosen for corrosion resistance.

Read comparison
Inconel 600
Inconel 625

Inconel 600 vs Inconel 625

Inconel 600 is a plain nickel-chromium-iron alloy with about 15.5% chromium and 8% iron.

Read comparison
Hastelloy C-22
Hastelloy C-276

Hastelloy C-22 vs Hastelloy C-276

Hastelloy C-22 has more chromium (about 22%) and less molybdenum (13%) than C-276 (15.5% Cr, 16% Mo), which makes it better in oxidising conditions.

Read comparison
Monel 400
Monel K-500

Monel 400 vs Monel K-500

Monel K-500 is Monel 400 with about 2.7% aluminium and 0.6% titanium added, so it can be age-hardened to much higher strength.

Read comparison
Duplex 2205
Super duplex 2507

Duplex 2205 vs Super Duplex 2507

Super duplex 2507 carries more chromium (25% against 22.5%), molybdenum (4% against 3.1%), nickel (7% against 5.5%) and nitrogen than duplex 2205, giving a PREN above 40 against about 35.

Read comparison
Inconel 625
Hastelloy C-276

Inconel vs Hastelloy

Inconel alloys are mostly nickel-chromium, built for oxidation resistance and strength at temperature.

Read comparison
Inconel 625
Incoloy 825

Inconel vs Incoloy

Inconel alloys are nickel-base, typically 50–76% nickel.

Read comparison
Titanium Grade 5
Inconel 718

Titanium vs Nickel Alloy

Titanium is a light metal (about 4.5 g/cm³) with a hexagonal crystal structure.

Read comparison
Inconel 625
Hastelloy C-276

Inconel 625 vs Hastelloy C-276

Inconel 625 carries about 21.5% chromium, 9% molybdenum and 3.6% niobium.

Read comparison
Inconel 600
Inconel 601

Inconel 600 vs Inconel 601

Inconel 600 is about 15.5% chromium and 8% iron.

Read comparison
Inconel 600
Inconel 690

Inconel 600 vs Inconel 690

Inconel 690 has about 29% chromium against about 15.5% in Inconel 600.

Read comparison
Incoloy 825
Inconel 625

Incoloy 825 vs Inconel 625

Incoloy 825 is an iron-nickel-chromium alloy with about 42% nickel, 30% iron, 3% molybdenum and 2% copper.

Read comparison
Hastelloy X
Haynes 230

Hastelloy X vs Haynes 230

Hastelloy X has about 22% chromium, 18.5% iron and 9% molybdenum.

Read comparison
Hastelloy B-2
Hastelloy C-276

Hastelloy B-2 vs C-276

Hastelloy B-2 is nickel with about 28% molybdenum and almost no chromium.

Read comparison
Super duplex 2507
Super duplex S32760

Super Duplex 2507 vs S32760

Both are super duplex stainless steels with about 25% chromium and 7% nickel.

Read comparison
Titanium Grade 2
Titanium Grade 5

Titanium Grade 2 vs Grade 5

Titanium Grade 2 is commercially pure titanium.

Read comparison
Nimonic 75
Nimonic 80A

Nimonic 75 vs Nimonic 80a

Both are nickel with about 20% chromium.

Read comparison
Inconel 718
Inconel 706

Inconel 718 vs Inconel 706

Inconel 718 has about 18.5% iron, 19% chromium, 5% niobium and 3% molybdenum.

Read comparison
Incoloy 825
Incoloy 925

Incoloy 825 vs Incoloy 925

Incoloy 925 is the age-hardenable version of 825.

Read comparison
Titanium Grade 2
Titanium Grade 7

Titanium Grade 2 vs Grade 7

Titanium Grade 7 is Grade 2 with about 0.15% palladium added for resistance to reducing acids.

Read comparison

Interactive

Compare Any Two Grades

Pick two grades to see their nominal composition side by side and the elements that separate them.

Also available as a standalone alloy comparison tool.

Questions

FAQ

Why compare nickel alloy grades?

Because grades that look identical can differ by several points of iron, molybdenum, niobium or chromium, which changes both their value and their melting route.

Can XRF tell these grades apart?

In most pairs, yes. Each comparison lists the XRF-visible elements that separate the two grades, and flags where light elements need OES or a lab.

Not Sure Which Grade You Have?

Send us photographs, markings or readings and we’ll review your enquiry.

Send Enquiry
Chat on WhatsApp